Polymer Property : Tensile Modulus = 0.217 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.217 GPa
31.5 ksi
ASTM D638
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound  (discontinued **)
This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company