Polymer Property : Tensile Modulus = 0.0580 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 0.0580 GPa
8.41 ksi
ISO 527
Lubrizol ESTANE® GP95AB Ester Based Thermoplastic Polyurethane
Type: Estane® GP 95AB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, animal identification tagsAvailable in ..
Tensile Modulus 0.0580 GPa
8.41 ksi
1 mm/min
Arkema Group Pebax® MX 1205 SN 01 Polyether Block Amide (PEBA) (Conditioned)
POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness..