Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.0269 GPa | 3.90 ksi | (0.2 in/min), Molded Properties; ASTM D638 |
ExxonMobil Escorene™ UL 53019CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 53019CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent.. |