Polymer Property : K Factor (ISO) = 4.3 µm/km Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K Factor (ISO) 4.3 µm/km

@Temperature 200 °C
4.3 µm/km

@Temperature 392 °F
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced
Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv..