Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 4.3 µm/km @Temperature 200 °C |
4.3 µm/km @Temperature 392 °F |
|
Wolf Kunststoff ZEDEX® ZX-530EL3 066 Polymer Alloy, Carbon Fiber Reinforced Main Characteristics: Low thermal expansion; High rigidity; High yield stress; High wear resistance; Low friction; Stress ResistantApplications: Chemical Engineering; Laboratory Technology; Automitv.. |