Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 3.6 µm/km @Temperature 200 °C |
3.6 µm/km @Temperature 392 °F |
|
Wolf Kunststoff ZEDEX® ZX-324VMT A3B PEEK, Fiber Reinforced Main Characteristics: Maximum rigidity; Very good wear resistance; Low stick-slip tendency; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInfor.. |