Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K Factor (ISO) | 3.4 µm/km @Temperature 20.0 °C |
3.4 µm/km @Temperature 68.0 °F |
|
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut.. |