Mechanical Properties Metric English Comments
K Factor (ISO) 1.4 µm/km

@Temperature 100 °C
1.4 µm/km

@Temperature 212 °F
Wolf Kunststoff ZEDEX® ZX-324V1T A3H PEEK Polymer, Reinforced
Main Characteristics: High resilience; High elasticity; Low permanent deformation; Stress resistant; High strength at temperatures above 140 ° CApplications: Shipbuilding; Chemical Engineering; Aut..
K Factor (ISO) 1.4 µm/km

@Temperature 100 °C
1.4 µm/km

@Temperature 212 °F
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified
Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex