Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 97.9 MPa | 14200 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 GF17 IM2 L 17% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 17% Filler by WeightAdditive: Lubricant and Impact ModifierFeatures: Lubricant and Impact ModifiedInformatio.. |
|||
Tensile Strength, Yield | 97.9 MPa | 14200 psi | ASTM D638 |
Techmer ES Luriblend® PSU GF20 TL5 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: PTFE LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 97.9 MPa | 14200 psi | ASTM D638 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Yield | 97.9 MPa | 14200 psi | ASTM 638 |
PlastxWorld CEVIAN® SKG30 30% GF ABS Glass fiber reinforced, heat resistant and flame retarded ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by Plast.. |
|||
Tensile Strength, Yield | 97.9 MPa | 14200 psi | ASTM D638 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Yield | 97.9 MPa | 14200 psi | ASTM D638 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Yield | 97.9 MPa | 14200 psi | ASTM D638 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Yield | 97.9 MPa | 14200 psi | ASTM D638 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Yield | 97.9 MPa | 14200 psi | ASTM D638 |
A. Schulman ComAlloy® E-14961 30% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Tensile Strength, Yield | 97.9 - 112 MPa | 14200 - 16200 psi | Average value: 107 MPa Grade Count:3 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |