Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 97.9 - 112 MPa | 14200 - 16200 psi | Average value: 107 MPa Grade Count:3 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |