Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 96.5 MPa | 14000 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Trilliant™ HC HC3320-0020 RS Natural Polybutylene Terephthalate (PBT) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Polymer Resources NY66-IM1-G13 Nylon 66, 13% Glass Reinforced, Toughened Nylon 66, 13% Glass Reinforced, Toughened and LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon g.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Polymer Resources NY66-M40 Nylon 66, 40% Mineral Filled Nylon 66, 40% Mineral Filled, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Polymer Resources NY66-M40-[color]-H Nylon 66, 40% Mineral Filled, Heat Stabilized Nylon 66, 40% Mineral Filled, Lubricated, Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon .. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Polymer Resources PPX-FRG20 Modified-PPO, V-1 Flame Retardant, 20% Glass Reinforced Modified-Polyphenylene Oxide, V-1 Flame Retardant, 20% Glass ReinforcedFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing condu.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Polymer Resources TP-GFMF1 Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame Retardant Polybutylene Terephthalate, 40% Glass/Mineral Reinforced, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ 81520 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM Data |
Dow Questra® EA503 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Polymer Resources NY66-IM1-G13-[color]-H Nylon 66, 13% Glass Reinforced, Toughened and Heat Stabilized Nylon 66, 13% Glass Reinforced, Toughened, Lubricated, and Heat StabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, tes.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Polymer Resources NY66-IMG13 Nylon, 13% Glass Reinforced, Impact Modified (DAM) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Polymer Resources PPX-FRG20 Modified PPO, UL 94 V-1, 20% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Tensile Strength, Yield | 96.5 - 110 MPa | 14000 - 16000 psi | Average value: 105 MPa Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D-638 |
Glastic T-160 Fiberglass-Reinforced Polyester Laminate Grade T-160 is a new, high-strength, heat-resistant laminate. This highly creep-resistant material is excellent for applications where electrically insulating materials are subject to physical load.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 GF13 SS10 BK 13/10% Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Stainless Steel Reinforcement, 13/10% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill® ABS GF30 A1 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightFeatures: Good FlowInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill® PA6 GF/B20 A3 BK 20% Glass Fiber/Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber/Glass Bead, 20% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance: .. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Star Plastics PCGF20 Molding Grade PC with 20% Glass Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill® PEEK 450 BK Availability: North AmericaForms: PelletsFeatures: High ViscosityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill® POM CO GF/M30 UV BK 30% Glass Milled/Glass Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Milled/Glass Fiber, 30% Filler by WeightAdditive: UV StabilizerFeatures: Copolymer and Chemically CoupledAppearance: BlackInforma.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES Plastiblend® PA6/ABS 1120 GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: Natural ColorInformation p.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES Statiblend® PA6/6 GF20 AS BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Lubricant, Antistatic and Heat StabilizerFeatures: Antistatic, Heat Stabilized and Lubricate.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES Electrablend® ABS CF15 FR BK 15% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 15% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 GF13 FR-N BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Westlake Plastics Tempalux® 5000 Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high heat resistance, high strength at elevated temperatures, hi.. |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Clariant Renol 66G15BL-195 Blue Nylon 66, 15% Glass Fiber Reinforced Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Clariant Renol PA213G13 Nylon 6, 13% Glass Fiber, Heat Stabilized, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-40FG-0100 40% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Asahi Kasei Thermylene® P6-40FG-0874 40% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Asahi Kasei Thermylene® P7-30FG-0684 30% Glass Fiber Reinforced, Heat and UV Stabilized Information provided by Asahi Thermofil |
|||
Tensile Strength, Yield | 96.5 MPa | 14000 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 GF15 FR-N 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized, Halog.. |