Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Trilliant™ HC HC3320-0020 RS Natural Polybutylene Terephthalate (PBT)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer PolyOne Corporation
Trade Name Trilliant™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Trilliant™ HC HC3320-0020 RS Natural Polybutylene Terephthalate (PBT).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead of the competition. When specified, Trilliant® compounds may incorporate agency rated materials that meet USP Class VI, FDA or ISO 10993 testing requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.018 cm/cm
0.018 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 96.5 MPa
14000 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 9.0 %
9.0 %
Type I, 51 mm/min; ASTM D638
Flexural Strength 162 MPa
23500 psi
ASTM D790
Flexural Modulus 6.14 GPa
891 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.899 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 216 - 232 °C
421 - 450 °F
Deflection Temperature at 0.46 MPa (66 psi) >= 218 °C

@Thickness 3.18 mm
>= 424 °F

@Thickness 0.125 in
Annealed; ASTM D648
Processing Properties Metric English Comments
Mold Temperature 48.9 - 65.6 °C
120 - 150 °F
Drying Temperature 93.3 °C
200 °F
Dry Time 3.00 hour
3.00 hour
Descriptive Properties Value Comments
Agency Ratings USP Class VI
Appearance Natural Color
Features Biocompatible
Good Chemical Resistance
Good Colorability
Specialty Grade
Filler / Reinforcement Glass Fiber Reinforcement, 20% Filler by Weight
Forms Pellets
Generic Material PBT
Generic Name Polybutylene Terephthalate (PBT)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Hospital Goods
Medical/Healthcare Applications