Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 910 - 958 MPa | 132000 - 139000 psi | Rp 0.2 |
Arcam Ti6Al4V Titanium Alloy Ti6Al4V is the most widely used titanium alloy and has numerous applications in the medical industry, aerospace, automotive and marine equipment industry. Ti6Al4V ELI features Extra Low Interstitial.. |