Arcam Ti6Al4V Titanium Alloy

Category Metal , Nonferrous Metal , Titanium Alloy
Manufacturer Arcam
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arcam Ti6Al4V Titanium Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ti6Al4V is the most widely used titanium alloy and has numerous applications in the medical industry, aerospace, automotive and marine equipment industry. Ti6Al4V ELI features Extra Low Interstitials, especially Iron and Oxygen, providing improved ductility and fracture resistance at cryogenic temperatures.Information provided by Stratasys®
Mechanical Properties Metric English Comments
Hardness, Rockwell C 30 - 35
30 - 35
Tensile Strength, Ultimate 972 - 1030 MPa
141000 - 149000 psi
Rm
Tensile Strength, Yield 910 - 958 MPa
132000 - 139000 psi
Rp 0.2
Elongation at Break 12 - 16 %
12 - 16 %
Modulus of Elasticity 120 GPa
17400 ksi
Fatigue Strength 600 MPa

@# of Cycles >=1.00e+7
87000 psi

@# of Cycles >=1.00e+7
Component Elements Properties Metric English Comments
Aluminum, Al 6.0 %
6.0 %
Carbon, C 0.0030 %
0.0030 %
Hydrogen, H 0.0030 %
0.0030 %
Iron, Fe 0.10 %
0.10 %
Nitrogen, N 0.010 %
0.010 %
Oxygen, O 0.15 %
0.15 %
Titanium, Ti 89.734 %
89.734 %
Vanadium, V 4.0 %
4.0 %