Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 641 MPa @Temperature 82.2 °C |
93000 psi @Temperature 180 °F |
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 3K PW Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Strength, Yield | 641 MPa @Temperature -53.9 °C |
93000 psi @Temperature -65.0 °F |
0° Direction, Dry; Vacuum/Oven Cured; ASTM D3039-95 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T300 3K PW Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Tensile Strength, Yield | 641 MPa @Strain 0.200 % |
93000 psi @Strain 0.200 % |
|
Haynes Ultimet® alloy, all-weld metal, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 641 MPa @Strain 0.200 % |
93000 psi @Strain 0.200 % |
|
Haynes Hastelloy® C-22® alloy, 10% cold worked sheet HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys an.. |
|||
Tensile Strength, Yield | 641 MPa | 93000 psi | |
Universal Wire Works 80SD-2 Steel Welding Wire Universal 80SD-2 is a manganese, molybdenum, silicon low alloy steel wire producing weld deposits of unusually high strength, ductility and impact properties. This alloy was developed for the weldin.. |
|||
Tensile Strength, Yield | 641 - 779 MPa | 93000 - 113000 psi | 0.2% offset |
Eagle Brass 762 Nickel Silver 12%, Extra Hard 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long s.. |
|||
Tensile Strength, Yield | 641 MPa @Strain 0.200 %, Temperature -18.0 °C |
93000 psi @Strain 0.200 %, Temperature -0.400 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H1150 (Age Hardened 621°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |
|||
Tensile Strength, Yield | 641 MPa | 93000 psi | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 20% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |