Material Notes:
Universal 80SD-2 is a manganese, molybdenum, silicon low alloy steel wire producing weld deposits of unusually high strength, ductility and impact properties. This alloy was developed for the welding of medium carbon and sulphur bearing free machining steels. When MIG welding use CO2 shielding gas. The amounts of manganese and silicon in this alloy provide good salvaging action in the weld pool resulting in sound, porosity-free weld.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 710 MPa
103000 psi
Tensile Strength, Yield 641 MPa
93000 psi
Elongation at Break 23 %
23 %
Charpy Impact 75.9 J

@Temperature -51.1 °C
56.0 ft-lb

@Temperature -60.0 °F
97.6 J

@Temperature -17.8 °C
72.0 ft-lb

@Temperature 0.000 °F
Component Elements Properties Metric English Comments
Carbon, C 0.11 %
0.11 %
Iron, Fe 96.8 %
96.8 %
As Remainder
Manganese, Mn 1.92 %
1.92 %
Molybdenum, Mo 0.50 %
0.50 %
Nickel, Ni 0.020 %
0.020 %
Phosphorous, P 0.012 %
0.012 %
Silicon, Si 0.65 %
0.65 %
Sulfur, S 0.017 %
0.017 %
Users viewing this material also viewed the following: