Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 882 MPa @Temperature 23.0 °C |
128000 psi @Temperature 73.4 °F |
0°, Conditioning: 23°C; ASTM D3039 |
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 3K High Strength Carbon Fiber Designation: C280T4; Twill 4x4Information provided by HexCel |
|||
Tensile Strength, Yield | 882 MPa @Strain 0.200 % |
128000 psi @Strain 0.200 % |
|
Carpenter BioDur™ CCM Plus™ Medical Implant Alloy, Annealed 1093°C 1 hr Data provided by Carpenter Technology Corporation.Annealing followed by water quench and low stress grinding prior to tensile testing.Medical Implant Alloy. Non-magnetic Co-Cr-Mo alloy exhibiting h.. |
|||
Tensile Strength, Yield | 882 MPa | 128000 psi | Hardened 1800°F, Tempered 1000°F |
ATI Allegheny Ludlum 410 Martensitic Stainless Steel Characteristics: superior wear resistance, hardenable, excellent corrosion resistance. Applications:cutlery, dental and surgical instruments, nozzles, valve parts, hardened steel ball and seats for.. |
|||
Tensile Strength, Yield | 882 MPa @Strain 0.200 % |
128000 psi @Strain 0.200 % |
typical |
ATI Allegheny Ludlum Martensitic Stainless Steel Type 410, Hardened + 538°C Temper Allegheny Ludlum Type 410 is a hardenable straight-chromium stainless steel which combines superior wear resistance of high carbon alloys with the excellent corrosion resistance of chromium stainles.. |