Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.79 - 60.1 MPa | 260 - 8710 psi | Average value: 18.5 MPa Grade Count:49 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |