Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1.79 - 57.4 MPa | 260 - 8330 psi | Average value: 33.9 MPa Grade Count:181 |
Overview of materials for PVC, Extruded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Extruded". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
Tensile Strength, Yield | 1.79 - 60.1 MPa | 260 - 8710 psi | Average value: 18.5 MPa Grade Count:49 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Yield | 1.79 MPa | 260 psi | 200%, post cured- 8 hours at 177°C; ASTM D412 |
Multibase C6-235 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 1.79 MPa | 260 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 3501-35-NT Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Ultra High MW, Ethylene Oxide SterilizableForms-PelletsProcessing-Extrusion, Injection MoldingAppe.. |