Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 862 MPa | >= 125000 psi | |
Niagara LaSalle Fatigue-Proof® Cold Finished Steel Bar Fatigue-Proof® has the high strength properties usually associated only with heat treated steels. It also has excellent machining characteristics, resistance to fatigue and corresponds to AISI Grad.. |
|||
Tensile Strength, Yield | 862 MPa | 125000 psi | |
Pacific Sintered Materials FX-233-T(HT) Infiltrated Alloy Steel Excellent combination of strength and shock resistance. Good for use in cams, pawls, sprockets and wear plates. Moderate tolerance control.All information provided by Pacific Sintered Metals. |
|||
Tensile Strength, Yield | 862 - 960 MPa | 125000 - 139000 psi | |
Materion Beryllium Nickel Strip - Alloy 360 MH2, Mill Hardened Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: Mill HardenedStress Relaxation-% Stress Remaining after 1000 hrs @ 100°C: 99%Stress Relaxation afte.. |
|||
Tensile Strength, Yield | 862 - 1210 MPa @Strain 0.200 % |
125000 - 175000 psi @Strain 0.200 % |
|
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Cold-Drawn and Aged Rod and Bar specifically. Other property values are typ.. |
|||
Tensile Strength, Yield | >= 862 MPa @Temperature 1075 °C, Time 14400 sec |
>= 125000 psi @Temperature 1967 °F, Time 4.00 hour |
|
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |
|||
Tensile Strength, Yield | >= 862 MPa @Temperature 1150 °C, Time 14400 sec |
>= 125000 psi @Temperature 2100 °F, Time 4.00 hour |
|
Schmolz + Bickenbach UGIMA® 630 Stainless Steel Bar Description: 630 UGIMA® is an improved machining martensitic precipitation hardenable grade produced only by Ugitech. It is identical in every way to standard type 630 (17-4), except with respect.. |
|||
Tensile Strength, Yield | 862 MPa | 125000 psi | |
Wingate Alloys Winco HCP 60 Induction Hardened Turned, Ground and Polished, Hard Chromium Plated Shafting A corrosive resistant hardened shafting.Winco HCP 60 is an induction hardened TGP shaft that is hard chrome plated and polished to a mirror finish of RMS 8 minimum. This hard chrome plated finish pr.. |
|||
Tensile Strength, Yield | >= 862 MPa | >= 125000 psi | |
Wingate Alloys Winco HCP Hard Chromium Plated Turned, Ground and Polished Shafting A corrosive resistant shafting for piston rod and hydraulic piston applications.Winco HCP introduces a new concept in turned, ground and polished, hard chromium plated bars. The hardness, toughness .. |
|||
Tensile Strength, Yield | 862 MPa @Strain 0.200 % |
125000 psi @Strain 0.200 % |
|
Carpenter MP35N* Ni-Co-Cr-Mo Alloy, 15% Cold Reduction + Aged 538°C (1000°F)/4hr/AC Data provided by Carpenter Technology Corporation.Carpenter MP35N alloy is a nonmagnetic, nickel-cobalt-chromium-molybdenum alloy possessing a unique combination of ultrahigh tensile strength, good .. |
|||
Tensile Strength, Yield | 862 MPa @Strain 0.200 % |
125000 psi @Strain 0.200 % |
|
ATI Allvac® 6-4 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal Data provided by Allvac.Applications: Blades, discs, rings, airframe, fasteners, components. Vessels, cases, hubs, forgings. Standard, rotor/premium grades. |
|||
Tensile Strength, Yield | 862 MPa @Strain 0.200 % |
125000 psi @Strain 0.200 % |
|
ATI Allvac® Astroloy Nickel Superalloy, Heat Treatment: 1163°C (2125°F) + Age Data provided by Allvac.Applications: Discs, rings, bolts for gas turbines. |
|||
Tensile Strength, Yield | 862 MPa | 125000 psi | Long. |
ATI Wah Chang 425™ Titanium Alloy, Annealed Bar 0.5 - 1.23 in. dia ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Tensile Strength, Yield | 862 MPa | 125000 psi | Long. |
ATI Wah Chang 425™ Titanium Alloy, Tubular Extruded, Mill Annealed ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p.. |
|||
Tensile Strength, Yield | 862 MPa @Strain 0.200 %, Temperature 316 °C |
125000 psi @Strain 0.200 %, Temperature 601 °F |
|
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |