Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Niagara LaSalle Fatigue-Proof® Cold Finished Steel Bar

Category Metal , Ferrous Metal , Carbon Steel , AISI 1000 Series Steel
Manufacturer Niagara LaSalle
Trade Name Fatigue-Proof®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niagara LaSalle Fatigue-Proof® Cold Finished Steel Bar.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fatigue-Proof® has the high strength properties usually associated only with heat treated steels. It also has excellent machining characteristics, resistance to fatigue and corresponds to AISI Grade 1144. From this special quality hot roll grade Fatigue-Proof® is made by various combinations of mechanical working and thermal treatment wear, and it minimizes distortion. Fatigue-Proof® is produced from a high manganese, resulfurized, silicon killed steel.Information provided by Niagra LaSalle Corporation
Mechanical Properties Metric English Comments
Hardness, Brinell >= 285
>= 285
Hardness, Rockwell C >= 30
>= 30
Tensile Strength >= 965 MPa
>= 140000 psi
Tensile Strength, Yield >= 862 MPa
>= 125000 psi
Elongation at Break >= 5.0 %
>= 5.0 %
Reduction of Area >= 15 %
>= 15 %
Component Elements Properties Metric English Comments
Carbon, C 0.40 - 0.48 %
0.40 - 0.48 %
Iron, Fe 96.79 - 97.86 %
96.79 - 97.86 %
as balance
Manganese, Mn 1.35 - 1.65 %
1.35 - 1.65 %
Phosphorous, P <= 0.40 %
<= 0.40 %
Silicon, Si 0.15 - 0.35 %
0.15 - 0.35 %
Sulfur, S 0.24 - 0.33 %
0.24 - 0.33 %
Users viewing this material also viewed the following: