Polymer Property : Tensile Strength, Yield = 80.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.552 MPa

@Strain 300 %
80.0 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP 1869 Thermoplastic Elastomer
Features: Monprene® TPE gels are softer than the shore A range of hardness. Monprene® TPE gels are high strength and high flow elastomers that may be used in the overmolding processes on poly..
Tensile Strength, Yield 0.552 MPa

@Strain 300 %
80.0 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® RT-3805M Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer..
Tensile Strength, Yield 0.552 MPa
80.0 psi
Resinlab® UR3010 Black Polyurethane Potting System
Resinlab™ UR 3010 Black is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro..
Tensile Strength, Yield 0.552 MPa
80.0 psi
Resinlab® UR3010 Clear Polyurethane Potting System
Resinlab™ UR 3010 Clear is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro..
Tensile Strength, Yield 0.552 - 900 MPa
80.0 - 131000 psi
Average value: 16.1 MPa Grade Count:244
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..
Tensile Strength, Yield 0.552 MPa

@Strain 300 %
80.0 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
PolyOne Synprene® ST-6105 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne Firs..