Polymer Property : Tensile Strength, Yield = 8.34 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 8.34 MPa
>= 1210 psi
Kazanorgsintez 107-18 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Tensile Strength, Yield >= 8.34 MPa
>= 1210 psi
Kazanorgsintez 107-19 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Tensile Strength, Yield >= 8.34 MPa
>= 1210 psi
Kazanorgsintez 107-20 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Tensile Strength, Yield >= 8.34 MPa
>= 1210 psi
Kazanorgsintez 107-22 Composition of Low Density Polyethylene, Crack-Proof
Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod..
Tensile Strength, Yield 8.34 MPa
1210 psi
ASTM D412
Teknor Apex Flexalloy® 9800-60 Polyvinyl Chloride Elastomer
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Oil Resistant, Ultra High MWUses- Footwear, Tubing, Gaskets, Tools (Power/Others), Hose, Wire and ..
Tensile Strength, Yield 8.34 MPa
1210 psi
at 100% elongation; ASTM D412
Lubrizol Estane® X-590A-31 Thermoplastic Polyurethane
Type: Estane® X-590A-31 is a Shore 91A, polyester grade without lubricant thermoplastic polyurethane (TPU). USP Class VI Certified.Uses: Extrusion, Film Blowing.Information Provided by The Lubrizo..
Tensile Strength, Yield 8.34 MPa
1210 psi
at 300% elongation; ASTM D412
Lubrizol Estane® CR180A Thermoplastic Polyurethane
Type: Estane® CR180A is a Shore 82A, polyether grade, calendering processible thermoplastic polyurethane (TPU). FDA approved (21 CFR 177.2600, 177.1680).Uses: Calendering, Molt roll processing.Inf..
Tensile Strength, Yield 8.34 MPa
1210 psi
100%; ASTM D412
Teknor Apex APEX® 2580-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Tensile Strength, Yield 8.34 - 20.7 MPa
1210 - 3000 psi
Average value: 12.3 MPa Grade Count:53
Overview of materials for Low Density Polyethylene (LDPE), Wire/Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Wire/Cable Grade". Each property range of values reported is minimum an..