Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.24 - 6.31 MPa | 760 - 915 psi | Average value: 5.69 MPa Grade Count:3 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate Copolymer (EVA), Extrusion/Coating Grade". Each property range of values reported.. |
|||
Tensile Strength, Yield | 5.24 MPa @Strain 300 % |
760 psi @Strain 300 % |
510 mm/min; ASTM D412A |
PolyOne Synprene® RT-5180 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom.. |
|||
Tensile Strength, Yield | 5.24 MPa | 760 psi | at 200%, no post cure- press cured for 5 minutes; ASTM D412 |
Multibase C6-570 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tensile Strength, Yield | 5.24 MPa | 760 psi | 100%; ASTM D412 |
Teknor Apex Flexalloy® 9100-65 Polyvinyl Chloride Elastomer Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTM Features: Good Flexibility, General Purpose, Ultra High MW, Recyclable, Good Thermal Stability, Good Weather.. |
|||
Tensile Strength, Yield | 5.24 MPa | 760 psi | ASTM D638 |
ExxonMobil Escorene® LD 728.61 Molding, extrusion and compounding resin Escorene Ultra LD 728.61 is a high vinyl acetate copolymer with low melting temperature and excellent strength properties and toughness.Availability: Latin America, North America and South America A.. |