Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.2 MPa
7570 psi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Rigid Extrusion 87736 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Strength, Yield 52.2 MPa

@Strain 0.200 %
7570 psi

@Strain 0.200 %
typical
ATI Allegheny Ludlum AL 611 Stainless Steel, UNS S30601
AL 611 alloys are low-carbon, silicon-containing, austenitic stainless steels. These alloys are typically used for applications in the chemical industry. The high silicon content provides them wit..