Material Notes:
AL 611 alloys are low-carbon, silicon-containing, austenitic stainless steels. These alloys are typically used for applications in the chemical industry. The high silicon content provides them with very good resistance to oxidizing environments, such as concentrated nitric acid, over a wide range of temperatures. Because of its higher alloy content, AL 611 material will be more resistant to highly concentrated nitric acid than AL 610 alloyInformation provided by Allegheny Ludlum
Physical Properties Metric English Comments
Density 7.589 g/cc
0.2742 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell B 91
91
Typical
Tensile Strength, Ultimate 710 MPa
103000 psi
Typical
Tensile Strength, Yield 52.2 MPa

@Strain 0.200 %
7570 psi

@Strain 0.200 %
typical
Elongation at Break 63 %
63 %
typical in 2"
Component Elements Properties Metric English Comments
Carbon, C 0.015 %
0.015 %
Chromium, Cr 17 - 18 %
17 - 18 %
Copper, Cu 0.35 %
0.35 %
Iron, Fe 58 - 60 %
58 - 60 %
as balance
Manganese, Mn 0.50 - 0.80 %
0.50 - 0.80 %
Molybdenum, Mo 0.20 %
0.20 %
Nickel, Ni 17 - 18 %
17 - 18 %
Nitrogen, N 0.050 %
0.050 %
Phosphorous, P 0.030 %
0.030 %
Silicon, Si 5.0 - 5.6 %
5.0 - 5.6 %
Sulfur, S 0.013 %
0.013 %