Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 738 MPa | >= 107000 psi | 0.2% offset |
Eagle Brass 64725 MAX251C, Extra Spring Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In.. |
|||
Tensile Strength, Yield | 738 - 814 MPa | 107000 - 118000 psi | 0.2% offset |
Eagle Brass 770 Nickel Silver 18%, Spring 770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi.. |
|||
Tensile Strength, Yield | 738 MPa @Strain 0.200 %, Temperature 538 °C |
107000 psi @Strain 0.200 %, Temperature 1000 °F |
|
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F)) Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope.. |
|||
Tensile Strength, Yield | 738 MPa @Strain 0.200 %, Temperature -73.0 °C |
107000 psi @Strain 0.200 %, Temperature -99.4 °F |
|
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 20% Cold Work Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®.. |