Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 107000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 740 MPa
>= 107000 psi
MetalTek MTEK 115 Martensitic Stainless Steel
Information provided by MetalTek
Tensile Strength, Yield 740 MPa

@Strain 0.200 %,
Temperature 540 °C
107000 psi

@Strain 0.200 %,
Temperature 1000 °F
Haynes 25 alloy, cold worked sheet, 15 % cold reduction
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield >= 740 MPa
>= 107000 psi
SSAB Tunnplat Domex® 740XP Extra High-strength Cold-forming Steel
Extra High-strength Cold-forming Steel, HSLACharacteristics: Domex® is the brand name of hot rolled products from SSAB Tunnplat. Domex® cold-forming steels are modern structural steels. Gene..
Tensile Strength, Yield 741 MPa

@Temperature 23.0 °C
107000 psi

@Temperature 73.4 °F
0°, Conditioning: 23°C; ASTM D3039
Hexcel® HexPly® M49 120°C Curing Epoxy Matrix, 6K High Strength Carbon
Fiber Designation: C370S5, Satin weave, 5HInformation provided by HexCel
Tensile Strength, Yield >= 738 MPa
>= 107000 psi
0.2% offset
Eagle Brass 64725 MAX251C, Extra Spring
Max 251c has an excellent balance in hardness, formability and conductivity. Typical uses include lead frames, circuit breakers, connectors, electrical springs, contact terminals, and fuse clips.In..
Tensile Strength, Yield 738 - 814 MPa
107000 - 118000 psi
0.2% offset
Eagle Brass 770 Nickel Silver 18%, Spring
770 has good cold forming properties, is tarnish resistant and has very good spring properties. 770 does not become subject to embrittlement at lower temperature and it has excellent corrosion resi..
Tensile Strength, Yield 738 MPa

@Strain 0.200 %,
Temperature 538 °C
107000 psi

@Strain 0.200 %,
Temperature 1000 °F
Carpenter Custom 455® Stainless Steel, Condition H1000 (Age Hardened 538°C (1000°F))
Data provided by Carpenter Technology Corporation.Recognizing the need for high-strength alloys with good corrosion resistance to atmospheric environments, the Carpenter Research Laboratory develope..
Tensile Strength, Yield 738 MPa

@Strain 0.200 %,
Temperature -73.0 °C
107000 psi

@Strain 0.200 %,
Temperature -99.4 °F
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 20% Cold Work
Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®..
Copyright © lookpolymers.com All Rights Reserved