Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 50.5 MPa | 7320 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion L1361 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 50.5 MPa | 7320 psi | 50 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® M205FC ABS Pellets, Injection Molding Grade Injection Molding grade for medical applications (e.g. inhalers, roller clamps, spikes, etc.)/ Biocompatible with up to 30 days human contact duration according to USP Class VI and ISO 10993-1. Food.. |
|||
Tensile Strength, Yield | 50.5 MPa | 7320 psi | ASTM D-638 |
Axiall LR-5009 Rigid PVC, Molding, All Colors Georgia Gulf LR-5009 is an economical high flow rigid PVC fittings compound designed for multi-cavity molds and large diameter fittings. This compound is characterized by excellent process ability,.. |