Mechanical Properties Metric English Comments
Tensile Strength, Yield 707 - 821 MPa
102000 - 119000 psi
1"x 0.020" Aramid/Glass
Glastic GoldMemberâ„¢ Pre-tensioned Fiber Reinforcements
GoldMemberâ„¢ fiber reinforcements are available in ribbon, tape and rounds that can be applied to thermoplastics and thermoset plastics, as well as wood and metals to add strength, rigidity, and..
Tensile Strength, Yield 707 MPa

@Treatment Temp. 760 °C,
Time 1.44e+7 sec
103000 psi

@Treatment Temp. 1400 °F,
Time 4000 hour
0.2%. Room temp test after thermal exposure
Haynes 282® Nickel Alloy Plate, Solution Annealed and Age-Hardened, after long term high temperature exposure
Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b..
Tensile Strength, Yield 707 MPa
103000 psi
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy
The higher tungsten content of Stellite alloy 4 gives improved high temperature properties and an increase in abrasive wear resistance over Stellite alloy 6, but not as good as Stellite alloy 12 or ..