Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 70.2 MPa | 10200 psi | ASTM D638M |
DSM Somos® ProtoTherm™ 12120 Water-resistant resin for stereolithography, UV Postcure DescriptionDSM Somos® 12120 is a liquid photopolymer that produces strong, high temperature tolerant, water-resistant parts. Parts created with Somos® 12120 have a cherry-red appearance which tur.. |
|||
Tensile Strength, Yield | 70.2 MPa | 10200 psi | ASTM D412 |
C.O.I.M. LARIPUR® LPR6325 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
Tensile Strength, Yield | 70.2 MPa | 10200 psi | ASTM D638 |
Cheng Yu Plastic A703G2 ABS 20% Glass Fiber Reinforced |