Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.483 MPa | 70.0 psi | at 150% elongation, maximum |
Dow Corning SILASTIC® 9280/30 KIT PARTS A&B 40 Durometer, 2-part, 1 to 1 mix, translucent Liquid Silicone Rubber.Information provided by Dow Corning |