Dow Corning SILASTIC® 9280/30 KIT PARTS A&B

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® 9280/30 KIT PARTS A&B.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
40 Durometer, 2-part, 1 to 1 mix, translucent Liquid Silicone Rubber.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity <= 1.14 g/cc

@Temperature 25.0 °C
<= 1.14 g/cc

@Temperature 77.0 °F
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore A 27
27
Tensile Strength, Ultimate 9.79 MPa
1420 psi
Tensile Strength, Yield 0.483 MPa
70.0 psi
at 150% elongation, maximum
Elongation at Break 970 %
970 %
Tear Strength 32.4 kN/m
185 pli
Compression Set 38 %
38 %
Electrical Properties Metric English Comments
Volume Resistivity 6.60e+14 ohm-cm
6.60e+14 ohm-cm
Dielectric Constant 2.9

@Frequency 100000 Hz
2.9

@Frequency 100000 Hz
2.93

@Frequency 100 Hz
2.93

@Frequency 100 Hz
Dielectric Strength 18.1 kV/mm
460 kV/in
Dissipation Factor 0.0025

@Frequency 100000 Hz
0.0025

@Frequency 100000 Hz
0.0059

@Frequency 100 Hz
0.0059

@Frequency 100 Hz
Processing Properties Metric English Comments
Pot Life 1440 min
1440 min
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Appearance translucent
Mix Ratio (X:1) 100
Base to Catalyst ETN