Tensile Strength, Yield 7.315 MPa
1061 psi
10% change after 168 hours @ 200°C; ASTM D412
Precision Polymer Engineering S71U Silicone Rubber
Translucent Silicone Rubber, 70-75 °IRHD. Platinum cured Silicone rubber having both methyl and vinyl substituent groups on the polymer chain. Silicone compound in conformity with the requirement..