Polymer Property : Tensile Strength, Yield = 6642 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 45.79 MPa
6642 psi
chs 2 in/min; ASTM D638
Diamond Polymers ASA 91802
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 45.79 MPa
6642 psi
chs 2 in/min; ASTM D638
Diamond Polymers ASA TW-23V
Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc.