Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 45.79 MPa | 6642 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA 91802 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 45.79 MPa | 6642 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA TW-23V Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |