Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.56 MPa | 661 psi | ASTM D412 |
Elastocon TPE Technologies Elastocon® STK55PA Thermoplastic Elastomer Elastocon® STK55PA thermoplastic elastomer has been developed for applications that require soft rubber-like properties and a good surface finish. Elastocon® STK55PA is well suited for consumer go.. |