Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 66.2 MPa | 9600 psi | ASTM D638 |
Polymer Resources PC-HH Polycarbonate, High Heat Polycarbonate, High HeatProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resource.. |
|||
Tensile Strength, Yield | 66.2 MPa | 9600 psi | ASTM D638 |
Polymer Resources PC-HH-UV Polycarbonate, High Heat, UV-stabilized Polycarbonate, High Heat, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by P.. |
|||
Tensile Strength, Yield | 66.2 MPa | 9600 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® PCGF110 Polycarbonate, 10% Glass-Filled High modulus 10% glass-filled polycarbonate, V2-rated, general purposeAll information provided by LTL Color Compounders, Inc. |
|||
Tensile Strength, Yield | 66.2 MPa | 9600 psi | ASTM D638 |
Techmer ES HiFill® TPU GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 66.2 MPa | 9600 psi | ASTM D638 |
Washington Penn Homopolymer Polypropylene 20% Glass Reinforced Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. .. |
|||
Tensile Strength, Yield | 66.2 MPa | 9600 psi | ASTM D638 |
Westlake Plastics Zelux® 10% GF Polycarbonate 10% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Tensile Strength, Yield | 66.2 MPa | 9600 psi | 2.0 in/min; ASTM D638 |
LTL Color Compounds ColorFast® FRPC310 Polycarbonate, Flame-Retarded V0-rated 10% glass-filled polycarbonate, excellent impact strengthAll information provided by LTL Color Compounders, Inc. |