Polymer Property : Tensile Strength, Yield = 65.07 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.07 MPa
9438 psi
ASTM D638
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Yield 65.07 MPa
9438 psi
ASTM D638
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Yield 65.07 MPa
9438 psi
ASTM D638
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Yield 65.07 MPa
9438 psi
ASTM D638
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Yield 65.07 MPa
9438 psi
ASTM D638
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
Tensile Strength, Yield 65.07 MPa
9438 psi
ASTM D638
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.