Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.5 MPa
6160 psi
200°C for 1,000 hrs
Fujipoly Industries Sarcon® 20GHR Thin-Film GHR
Sarcon HR is Fujipolys originally developed High Heat Conductive Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Sarcon GHR is a composite of ..
Tensile Strength, Yield 42.5 MPa

@Temperature 115 - 145 °C,
Time 1.80e+7 sec
6160 psi

@Temperature 239 - 293 °F,
Time 5000 hour
5 [mm/min], 50% Loss of Tensile Strength; ICE 216
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Tensile Strength, Yield 42.5 MPa

@Temperature 100 - 120 °C,
Time 7.20e+7 sec
6160 psi

@Temperature 212 - 248 °F,
Time 20000 hour
5 [mm/min], 50% Loss of Tensile Strength; ICE 216
Akro-Plastic Akromid® A3 (2414) PA 6.6 Dry
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Tensile Strength, Yield 42.5 MPa

@Temperature 100 - 140 °C,
Time 1.80e+7 sec
6160 psi

@Temperature 212 - 284 °F,
Time 5000 hour
5 [mm/min], 50% Loss of Tensile Strength; ICE 216
Akro-Plastic Akromid® B3 (2500) PA 6 Dry
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Tensile Strength, Yield 42.5 MPa

@Temperature 90.0 - 120 °C,
Time 7.20e+7 sec
6160 psi

@Temperature 194 - 248 °F,
Time 20000 hour
5 [mm/min], 50% Loss of Tensile Strength; ICE 216
Akro-Plastic Akromid® B3 (2500) PA 6 Dry
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..