Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 421 MPa @Strain 0.200 %, Temperature 538 °C |
61100 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Ultimet® alloy, all-weld metal, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 421 MPa @Strain 0.200 % |
61100 psi @Strain 0.200 % |
|
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.125 in (3.2 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.125 inch sheet. Other property values are typical of INCONEL® alloy 686.Data provided by the manufacture.. |