Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 421 MPa @Temperature 23.9 °C |
61000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 Type 1 |
Park Electrochemical Nelcote® V-303 Polyimide Prepreg, 7781 E-Glass Reinforced Nelcote® V-303 is non-MDA condensation polyimide prepreg with a service temperature of 600°F.Key Features and Benefits:600°F maximum service temperatureGood electrical properties for RF applicati.. |
|||
Tensile Strength, Yield | 421 MPa @Strain 0.200 %, Temperature 538 °C |
61100 psi @Strain 0.200 %, Temperature 1000 °F |
|
Haynes Ultimet® alloy, all-weld metal, SMAW weld Co content as balance, excellent corrosion resistance, outstanding wear resistance, high tensile strength combined with excellent impact toughness and ductility. Ideal welding material with exceptio.. |
|||
Tensile Strength, Yield | 421 - 517 MPa | 61000 - 75000 psi | 0.2% offset |
Eagle Brass 510 Phosphor Bronzes 5% A, 3/4 Hard Alloy C510 is an alloy with good strength, formability and stress relaxation characteristics, and solderability. Applications include electronic parts, springs, switches, contacts and fasteners.Info.. |
|||
Tensile Strength, Yield | 421 MPa @Strain 0.200 % |
61100 psi @Strain 0.200 % |
|
Special Metals INCONEL® 686 Nickel Superalloy (UNS N06686) Sheet 0.125 in (3.2 mm) Tensile strength (ultimate and yield) and elongation values reported here are typical for 0.125 inch sheet. Other property values are typical of INCONEL® alloy 686.Data provided by the manufacture.. |