Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.17 MPa | 605 psi | ASTM D412 |
Polymax® Maxelast® P1957TB TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Strength, Yield | 4.17 MPa @Strain 100 % |
605 psi @Strain 100 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL-0203-12 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) |