Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Elastamax™ XL-0203-12 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax™ XL-0203-12 Styrene Butadiene Block Copolymer (SBC)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 70

@Time 5.00 sec
70

@Time 0.00139 hour
ASTM D2240
Tensile Strength at Break 6.48 MPa
940 psi
510 mm/min; ASTM D412A
Tensile Strength, Yield 4.17 MPa

@Strain 100 %
605 psi

@Strain 100 %
510 mm/min; ASTM D412A
Elongation at Break 260 %
260 %
510 mm/min; ASTM D412A
Tear Strength 26.3 kN/m
150 pli
Die C, 510 mm/min; ASTM D624
Descriptive Properties Value Comments
Features General Purpose
Forms Pellets
Generic Name Styrene Butadiene Block Copolymer (SBC)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Consumer Applications
General Purpose
Overmolding
Copyright © lookpolymers.com All Rights Reserved