Tensile Strength, Yield 6.14 MPa
890 psi
chs 20 in/min; ASTM D412
Network Polymers Softflex® 5300
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Tensile Strength, Yield 6.14 MPa
890 psi
chs 20 in/min; ASTM D412
Network Polymers Softflex® 5500
Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc.
Tensile Strength, Yield 6.14 MPa
890 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
PolyOne Synprene® RT-5165 Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalIgnition ResistantApplications:Multi-PurposeMarket:Building and ConstructionConsumer GoodsIndustrialProcessing Method:Injection Mo..