Mechanical Properties Metric English Comments
Tensile Strength, Yield 4.08 MPa
592 psi
ASTM D412
Polymax® Maxelast® S4740 TPE, PS Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong ..