Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.08 MPa | 592 psi | ASTM D412 |
Polymax® Maxelast® S4740 TPE, PS Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesSporting GoodsInformation from Alliance Polymers & Services, Distributor of Nantong .. |