Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 58.3 MPa
8450 psi
ASTM D638
Ensinger Tecaform™ UD Blue Ultra Detectable Acetal Copolymer (POM)
TECAFORM® UD Blue is an Ultra Detectable acetal copolymer designed specifically for applications in the food industry. High speed food production lines detect particulate matter in the food product..