Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecaform™ UD Blue Ultra Detectable Acetal Copolymer (POM)

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer Ensinger
Trade Name Tecaform™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecaform™ UD Blue Ultra Detectable Acetal Copolymer (POM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TECAFORM® UD Blue is an Ultra Detectable acetal copolymer designed specifically for applications in the food industry. High speed food production lines detect particulate matter in the food product one of three ways; Using optical scanners, metal detection equipment, or X-ray equipment TECAFORM® UD Blue is the first engineering thermoplastic that will show up regardless of the scanning method used.Features:Food contact blue in colorHigh visibility of fillerDetectable by X-ray or metal detection equipmentPlastic chunks as small as 3mm thick detected using standard metal detection equipmentPlastic shavings to 1mm thick detected using standard metal detection equipmentEasily machined
Physical Properties Metric English Comments
Specific Gravity 1.61 g/cc
1.61 g/cc
ASTM D790
Mechanical Properties Metric English Comments
Hardness, Rockwell M 89
89
ASTM D785
Tensile Strength, Yield 58.3 MPa
8450 psi
ASTM D638
Elongation at Break 7.9 %
7.9 %
ASTM D638
Tensile Modulus 2.76 GPa
400 ksi
ASTM D638
Flexural Strength 95.01 MPa
13780 psi
ASTM D790
Flexural Modulus 3.16 GPa
459 ksi
ASTM D790
Compressive Strength 18.9 MPa
2740 psi
at 1% deformation; ASTM D695
87.22 MPa
12650 psi
at 10% deformation; ASTM D695
Compressive Modulus 1.82 GPa
264 ksi
ASTM D695
Izod Impact, Unnotched 0.363 J/cm
0.680 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
ASTM D3418
Maximum Service Temperature, Air 100 °C
212 °F
Long Term; UL746B