Polymer Property : Tensile Strength, Yield = 553.39 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.8155 MPa

@Treatment Temp. 200 °C,
Time 252000 sec
553.39 psi

@Treatment Temp. 392 °F,
Time 70.0 hour
Heat Aging; ASTM D573
Vicone High Performance Rubber VicoSil™ C303Q-GY High Performance Silicone Rubber
Information provided by Vicone